Corundum Hi-Intensity & Low Cement,
Refactory Pouring Material
ZM-18 S
1700 C
3.00gcm3
AL2O3>92%, SiO2<4%
110 C x 24h > 13 M Pa
1100 C x 3h > 13 M Pa
110 C x 24h > 13 M Pa
1100 C x 3h > 13 M Pa
1100 C x 3h > -0.10% ~ -0.30%
5.0% ~ 6.0%